Kummandla we-ultra-precision metrology, imfezeko yePlatform yeCandelo leGranite ayinakuxoxisana. Ngoxa i-ZHHIMG® ibambelela kwimigangatho ephezulu yokuvelisa kunye nokuhlola-eqinisekisiwe yi-ISO 9001, 45001, kunye ne-14001-akukho nto yendalo okanye inkqubo ekhuselekile ngokupheleleyo kwimiba enokubakho. Ukuzinikela kwethu asikokuvelisa nje umgangatho, kodwa kukwabelana ngobuchule obufunekayo ukuze siqonde kwaye sigcine loo mgangatho.

Esi sikhokelo sichaza imiba eqhelekileyo enokuchaphazela iiPlatform zeGranite ezichanekileyo kunye neendlela zobuchwephesha ezisetyenziselwa ukunciphisa okanye ukuzilungisa, ukuqhuba ukuphuculwa komsebenzi okuqhubekayo.

1. Ukulahleka kweFlatness okanye ukuchaneka kweJometri

Umsebenzi ophambili weqonga legranite kukubonelela ngenqwelomoya eyinyani egqibeleleyo. Ilahleko yokucaba sesona siphene sibaluleke kakhulu, esisoloko sibangelwa yimiba yangaphandle kunokusilela kwezinto.

Unobangela kunye neMpembelelo:

Izizathu ezibini eziphambili ziyinkxaso engafanelekanga (iqonga aliphumli kumanqaku alo achaziweyo amathathu aphambili, okukhokelela ekuphambukeni) okanye umonakalo womzimba (impembelelo enzima okanye ukutsala izinto ezinzima emhlabeni wonke, kubangela ukukrazula kwendawo okanye ukunxiba).

Uphuculo kunye neendlela zokunciphisa:

  • Ukulinganisa kwakhona kunye neNkxaso: Khangela ngokukhawuleza ukufakwa kweqonga. Isiseko kufuneka silandele ngokungqongqo umgaqo-siseko wokuxhasa amanqaku amathathu ukuqinisekisa ukuba ubunzima begranite buphumla ngokukhululekileyo kwaye abuxhomekeke kumandla okuguqula. Ukubhekisa kwizikhokelo zethu zomgangatho kubalulekile.
  • I-Surface Re-Lapping: Ukuba ukutenxa kungaphezulu kokunyamezelana (umzkl, iBakala 00), iqonga elo kufuneka liphindwe ngobuchwephesha (re-ground-ground). Le nkqubo idinga izixhobo ezikhethekileyo kunye nobuchule bamagcisa amashumi eminyaka yamava, njengalawo ase-ZHHIMG®, abanokubuyisela umgangatho wokuchaneka kwejometri yasekuqaleni.
  • Khusela kwiMpembelelo: Sebenzisa iiprothokholi zokusebenza ezingqongqo ukuthintela izixhobo ezinzima okanye izixhobo ukuba zingawiswa okanye zirhuqwe, ukukhusela umphezulu ekunxityweni kwendawo.

2. Iziphene zokuThabisa: Ukungcola kunye nokuguqulwa kombala

Ngelixa kungachaphazeli ngokuthe ngqo ukuchaneka komatshini osisiseko, iziphene zokuthambisa zinokuphazamisa ukucoceka okufunekayo kwiindawo ezinje ngamagumbi acocekileyo okanye iilebhu eziphezulu.

Unobangela kunye neMpembelelo:

Igranite ngokwendalo inemingxuma. Ukungcola kwenzeka xa imichiza, i-oyile, okanye ulwelo olunebala elimibalabala luvunyelwa ukuba luhlale phezu komhlaba, lugqobhoze imingxunya. Ngelixa i-ZHHIMG® Black Granite ixhathisa kakhulu kwi-asidi kunye ne-alkali corrosion, ukungahoywa kuya kukhokelela kwi-mottling ebonakalayo.

Uphuculo kunye neendlela zokunciphisa:

  • Ukucocwa Kwangoko: Ukuchitheka kweoyile, igrisi, okanye imichiza edlayo kufuneka icocwe ngokukhawuleza kusetyenziswa amalaphu athambileyo, angenalutyana kunye nezicoci ezingathathi hlangothi nezivunyiweyo zegranite. Gwema ii-abrasive agents zokucoca.
  • Ukutywinwa (Ukugcinwa kwamaxesha athile): Ngelixa ivalwa ngokutywinwa ngexesha lokwenziwa kwemveliso, ukusetyenziswa kwamaxesha athile kobuchwephesha kwesitywini segranite esigqobhozayo kunokugcwalisa imingxuma emikroskopu, okonyusa kakhulu ukuchasana nokungcoliswa kwexesha elizayo kunye nokwenza lula ucoceko lwesiqhelo.

3. I-Edge Chipping okanye i-Cracking

Umonakalo kumaphethelo kunye neekona ngumcimbi oqhelekileyo ngexesha lokuthutha, ukufakela, okanye ukusetyenziswa okunzima. Ngelixa i-edge chipping encinci ayifaki esichengeni indawo yokusebenza esembindini, iintanda ezinkulu zinokulinika iqonga lingasebenziseki.

Unobangela kunye neMpembelelo:

Uxinzelelo lwempembelelo ephezulu, ehlala igxininiswe kumda ongaxhaswanga ngexesha lokuhamba okanye ukuhamba, kunokubangela ukutshiza okanye, kwiimeko ezinzima, ukuqhekeka ngenxa yoxinzelelo lwamandla.

isiseko segranite esichanekileyo

Uphuculo kunye neendlela zokunciphisa:

  • UkuPhathwa okuKhuselekileyo: Soloko usebenzisa izixhobo zokuphakamisa ezifanelekileyo kunye neendawo zokurhweba ezikhuselekileyo. Ungaze uphakamise amaqonga amakhulu usebenzisa imiphetho engaxhaswanga.
  • Ukulungiswa kwe-Epoxy: Iitshiphusi ezincinci kwincam ezingabalulekanga okanye kwiikona zihlala zilungiswa ngobuchwephesha kusetyenziswa i-pigmented epoxy filler. Oku kubuyisela inkangeleko yezimonyo kwaye kuthintele ukuhlukana okuqhubekayo, nangona kungachaphazeli indawo yokulinganisa eqinisekisiweyo.
  • Ukukrazula umonakalo obunzima: Ukuba i-crack isasazeka kakhulu kwindawo yokulinganisa, ukunyaniseka kwesakhiwo kunye nokuzinza kuphazamisekile, kwaye iqonga kufuneka lisuswe ngokuqhelekileyo kwinkonzo.

E-ZHHIMG®, injongo yethu kukubonelela ngamacandelo anciphisa le miba ukusuka ekuqaleni, enkosi kwimathiriyeli yethu yoxinaniso oluphezulu (≈ 3100 kg/m³) kunye nokugqiba ngobuchule. Ngokuqonda ezi ziphene zinokwenzeka kunye nokulandela iindlela ezizezona zingcono zogcino kunye nomgangatho, abasebenzisi banokuqinisekisa ukuba iiPlatform zabo zeGranite ezichanekileyo zigcina ukuchaneka kweBanga loku-0 kumashumi eminyaka.